광학 코팅

ECLEAR Anti-Fog Coating Systems

이 기술 제품군의 ECLEAR 모델, 소재 구조, 적용 분야, 공정 범위 및 검증 요구사항을 확인하십시오.

비교 예시: 왼쪽은 김서림 방지 처리 표면, 오른쪽은 무처리 기준 시편입니다. 실제 성능은 시험 조건에 따라 달라집니다.
비교 예시: 왼쪽은 김서림 방지 처리 표면, 오른쪽은 무처리 기준 시편입니다. 실제 성능은 시험 조건에 따라 달라집니다.
대표 구조

소재 적층 구조의 구성.

층은 기능 순서로 표시되며 정확한 구조는 등급별로 달라집니다.

  1. 01FC route: prepared unprimed PC / thermally cured anti-fog layer
  2. 02FT route: PC / qualified hardcoat / plasma activation / hydrophilic anti-fog topcoat
  3. 03Application-specific edge, ink and masking zones
작동 원리

Hydrophilic control of condensation at the optical surface.

01Fog reduces visibility when condensed water forms many discrete droplets that scatter light. A hydrophilic anti-fog surface encourages the moisture to spread into a more continuous film, reducing droplet-driven scattering.

02Anti-fog is not one universal formulation. FC-100 is positioned for qualified unprimed polycarbonate, while FT-100 uses a different route for a plasma-activated hardcoated PC surface. Mixing the preparation routes can cause immediate or aged adhesion failure.

03Initial clarity is only the first screen. Cleaning, abrasion, skin oils, packaging contact, humidity cycling and time between plasma treatment and coating can determine whether anti-fog performance survives real use.

핵심 장점

적용 조건을 기준으로 평가한 성능.

장점은 실제 기재, 공정 및 최종 조립체에서 평가합니다.

01

Hydrophilic fog-management mechanism

02

Routes for both qualified unprimed PC and hardcoated PC

03

Designed for safety eyewear, shields and visor applications

04

Application support covering pretreatment, coating and cure

적합성 평가 절차

소재 정의부터 양산 적층 구조 승인까지.

승인 절차는 소재, 가공 경로 및 고객 생산 라인을 함께 연결합니다.

01Identify surface

Determine whether the PC is bare, primed, hardcoated, printed or metallized.

02Select route

Use the approved FC or FT preparation and activation sequence.

03Apply uniformly

Control wet film, drainage, edge zones, flash-off and thermal cure.

04Stress the surface

Run the agreed fog, cleaning, abrasion and conditioning sequence.

검증 항목

사양 승인 전에 확보할 검증 자료.

대표 기재, 공정 조건 및 노화 순서를 사용하십시오.

  • Defined hot-fog, cold-to-warm or customer-specific condensation test
  • Optical transmission and haze before, during and after conditioning
  • Adhesion to bare or activated hardcoated PC
  • Cleaning-agent, sweat, abrasion and packaging-contact durability
  • Appearance uniformity around edges, holes, masks and printed zones
대표 특성

모든 수치에는 시험 방법과 승인된 개정본이 필요합니다.

대표값은 선정에 활용하며 관리 규격은 승인된 TDS를 따릅니다.

특성대표값 / 범위관리 기준
MechanismHydrophilic water-film formationVisual and specified anti-fog test
FC-100 substrateQualified unprimed PCGrade-specific TDS
FT-100 substratePlasma-treated hardcoated PCGrade-specific TDS
CureThermal/process dependentApproved SOP

대표값은 보증 규격이 아닙니다. 최종 기준은 승인된 ECLEAR TDS와 고객 검증 결과를 따릅니다.

자주 묻는 질문

라인 시험 전에 엔지니어가 확인할 질문.

샘플 요청 전에 소재 역할, 계면 및 공정 범위를 정의하십시오.

Does an anti-fog coating repel water?+

Normally no. Hydrophilic anti-fog technology spreads condensed water; hydrophobic technology promotes beading and roll-off. They solve different moisture problems and must not be described as interchangeable.

Can FT-100 be coated directly on any hardcoat?+

No. The hardcoat chemistry, plasma energy, surface cleanliness and treatment-to-coating time must be validated as a system.

Can ECLEAR recommend a grade from an application description alone?+

A first shortlist is possible, but a production recommendation requires the substrate, layer construction, equipment, process sequence, test method and acceptance criteria. ECLEAR normally moves from requirement definition to laboratory matching, samples, line trial and a frozen approved specification.

Are the values shown on this page guaranteed specifications?+

No. Website values and constructions are selection guidance. Guaranteed limits, test conditions, packaging and shelf life are controlled only by the latest ECLEAR-approved TDS, quality agreement and customer qualification record.

권장 적용 분야

이 플랫폼을 평가하는 적용 분야.

각 적용에는 전체 적층 구조의 호환성과 라인 검증이 필요합니다.

Helmet visorsSafety eyewearFace shieldsProtective lensesOptical covers
공정 윈도우

관리해야 할 공정 변수.

하나의 명목 조건이 아니라 전체 공정 범위를 기록하십시오.

  • Do not substitute the FC and FT preparation routes.
  • For FT-100, validate hardcoat chemistry, plasma energy, treatment-to-coating time and surface cleanliness.
  • Control wet-film uniformity, flash-off, cure and handling after cure.
  • Use the customer-agreed fog test, conditioning and abrasion sequence.
선정 질문

선정에 필요한 정보.

이 정보로 ECLEAR가 적합한 등급과 검증 계획을 좁힐 수 있습니다.

  1. Q1Is the PC surface uncoated, primed, hardcoated, printed or metallized?
  2. Q2Is plasma treatment available and how is it controlled?
  3. Q3Which anti-fog standard and durability sequence must be met?
  4. Q4Will the coated surface contact cleaners, skin oils or packaging materials?
일반적인 고장 위험

체계적인 시험에서 조기에 드러나야 할 위험.

조기 고장 검사는 양산 확대 위험과 잘못된 소재 비교를 줄입니다.

!

Coating a hardcoat without the required activation step

!

Using an unspecified cleaner that changes hydrophilic performance

!

Blocking, print transfer or contamination during packaging

!

Treating one anti-fog grade description as a universal specification

다운로드 문서

관리되는 기술 문서.

선정한 ECLEAR 등급과 적용 분야의 최신 개정본을 요청하십시오.

ECLEAR Optics 원본 제품 페이지

대표 구조와 적용 개념은 소재 선정을 위한 정보입니다. 공급 여부, 구조, 성능 및 공정 조건은 등급별로 다르며 최신 ECLEAR 승인 TDS, 적용 시험 및 고객의 최종 승인에 따릅니다.

관련 제품

관련 소재 시스템.

동일한 적층 구조나 공정에서 이 제품과 상호 작용하는 인접 소재를 확인하십시오.

기술 상담

한 가지 소재가 아니라 전체 적층 구조를 검증하십시오.

정확한 제안을 위해 기재, 구조, 공정 및 합격 기준을 알려 주십시오.

프로젝트 시작